Revista: | Materials research |
Base de datos: | PERIÓDICA |
Número de sistema: | 000312392 |
ISSN: | 1516-1439 |
Autores: | Monteiro, Mauricio de Jesus1 Assuncao, Fernando Rizzo Chaoliu, Zeng2 |
Instituciones: | 1Pontificia Universidade Catolica do Rio de Janeiro, Departamento de Ciencias dos Materiais e Metalurgia, Rio de Janeiro. Brasil 2Chinese Academy of Sciences, Shenyang. China |
Año: | 1999 |
Periodo: | Jul |
Volumen: | 2 |
Número: | 3 |
Paginación: | 181-184 |
País: | Brasil |
Idioma: | Inglés |
Tipo de documento: | Artículo |
Enfoque: | Descriptivo |
Resumen en inglés | The oxidation of NiAl, NiAl-20at.%Fe and NiAl-30at.%Fe at 1000-1100 °C in air has been studied. Pure NiAl shows excellent oxidation resistance due to the formation of an Al2O3 layer. NiAl-20Fe also shows good oxidation resistance due to the formation of an Al2O3 scale on a b-phase substrate. Moreover, some nodules consisting of mixed oxides of Fe and Ni grow over the ductile g-phase surface incorporated to the b-phase substrate. NiAl-30Fe alloy undergoes a much faster oxidation due to the formation of a non-protective Fe and Ni-rich scale, which is extremely susceptible to spallation. The addition of Fe to NiAl is detrimental to its oxidation resistance |
Disciplinas: | Ingeniería, Química |
Palabras clave: | Ingeniería metalúrgica, Ingeniería química, Química industrial, Compuestos intermetálicos, Oxidación, Resistencia |
Keyword: | Engineering, Chemistry, Chemical engineering, Metallurgical engineering, Industrial chemistry, Chemical industry, Intermetallic compounds, Oxidation, Resistance |
Texto completo: | Texto completo (Ver HTML) |