Effects of thinning on diameter, heartwood, density and drying defects of Gmelina arborea



Título del documento: Effects of thinning on diameter, heartwood, density and drying defects of Gmelina arborea
Revista: Maderas : ciencia y tecnología
Base de datos:
Número de sistema: 000544646
ISSN: 0718-221X
Autors: 1
1
1
Institucions: 1Instituto Tecnológico de Costa Rica, Escuela de Ingeniería en Forestal, Cartago. Costa Rica
Any:
Període: Abr
Volum: 17
Número: 2
Paginació: 365-372
País: Chile
Idioma: Inglés
Resumen en inglés The effect of three levels thinning intensity in Gmelina arborea plantation on tree diameter, heartwood (diameter and percentage), wood density and drying defects (twist, crook, bow and check) was studied. Wood used for this study was obtained from eight-year-old plantations with thinning intensity of 60, 70 and 80% of initial density. Nine trees were selected from each trial. Results showed that tree diameter and wood density were similar in thinning intensity of 70 and 80%, but tree diameter from the plantation with 60% of thinning intensity was lower than plantation of 70 and 80%. Wood density of trees from 60% thinning intensity plantation was higher than 70 and 80%. Heartwood diameter and its percentage were the highest in 80% of thinning intensity. But not difference was found between 60 and 70% in heartwood (diameter and percentage). Finally, drying defects were not affected significantly by thinning intensity.
Keyword: Fast-growth,
Plantation wood,
Tree morphologic,
Wood density,
Wood properties
Text complet: Texto completo (Ver HTML) Texto completo (Ver PDF)